Pipa Baja ASTM A213
Item | Pipa/tabung baja paduan ASTM A213 T12 | |
Standar | ASTM A213, JIS G3462, JIS G3458, DIN17175, GB9948, GB 6479, lsp. | |
Bahan | T12, STBA22, 15CrMo. | |
Spesifikasi | Ketebalan tembok | 1 mm ~ 120 mm |
Dhiameter njaba | 6mm ~ 2500mm | |
dawa | 5.8m, 6m, 11.8m, 12m, utawa kaya sing dibutuhake. | |
lumahing | Dicet ireng, dilapisi PE. | |
Komposisi kimia | C:0.05~0.15, Si≤0.5, Mn:0.30~0.61, P≤0,025, S≤0,025, Mo:0,44~0,65, Kr:0,80-1,25 | |
Jangka rega | Mantan kerja, FOB, CIF, CFR, lsp. | |
Wektu Pembayaran | TT, LC, OA, D/P | |
Ekspor menyang | Singapura, Kanada, Indonesia, Korea, AS, Inggris, Thailand, Peru, Arab Saudi, Vietnam, Iran, India, Ukraina, Brasil, Afrika Kidul, lsp. | |
Wektu Pangiriman | Wektu Pangiriman: Ing 30 dina lan Gumantung saka jumlah pesenan sampeyan. | |
Paket | paket standar ekspor;kothak kayu bundled, cocog kanggo kabeh jinis transportasi, utawa dibutuhake | |
Aplikasi | 1) boiler, penukar panas;2) Petroleum;3) Aerospace;4) kimia;5) daya listrik;6) Militer. |
Komposisi Kimia Baja Paduan ASTM A213(%, maks)
Kelas Baja | Komposisi kimia% | ||||||||||||
C | Si | Mn | P, S maks | Cr | Mo | Ni Max | V | Al Max | W | B | Nb | N | |
T2 | 0.10~0.20 | 0.10~0.30 | 0.30~0.61 | 0,025 | 0.50~0.81 | 0.44~0.65 | – | – | – | – | – | – | – |
T11 | 0.05~0.15 | 0.50~1.00 | 0.30~0.60 | 0,025 | 1.00~1.50 | 0.44~0.65 | – | – | – | – | – | – | – |
T12 | 0.05~0.15 | Max 0,5 | 0.30~0.61 | 0,025 | 0.80~1.25 | 0.44~0.65 | – | – | – | – | – | – | – |
T22 | 0.05~0.15 | Max 0,5 | 0.30~0.60 | 0,025 | 1.90~2.60 | 0.87~1.13 | – | – | – | – | – | – | – |
T91 | 0.07~0.14 | 0.20~0.50 | 0.30~0.60 | 0.02 | 8.0~9.5 | 0.85~1.05 | 0.4 | 0.18~0.25 | 0.015 | – | – | 0.06~0.10 | 0.03~0.07 |
T92 | 0.07~0.13 | Max 0,5 | 0.30~0.60 | 0.02 | 8.5~9.5 | 0.30~0.60 | 0.4 | 0.15~0.25 | 0.015 | 1.50~2.00 | 0,001~0,006 | 0.04~0.09 | 0.03~0.07 |
Sifat Mekanik Baja Paduan ASTM A213:
Kelas Baja | Sifat Mekanik | |||
T. S | Y. P | Elongation | Kekerasan | |
T2 | ≥ 415MPa | ≥ 205MPa | ≥ 30% | 163HBW(85HRB) |
T11 | ≥ 415MPa | ≥ 205MPa | ≥ 30% | 163HBW(85HRB) |
T12 | ≥ 415MPa | ≥ 220MPa | ≥ 30% | 163HBW(85HRB) |
T22 | ≥ 415MPa | ≥ 205MPa | ≥ 30% | 163HBW(85HRB) |
T91 | ≥ 585MPa | ≥ 415MPa | ≥ 20% | 250HBW(25HRB) |
T92 | ≥ 620MPa | ≥ 440MPa | ≥ 20% | 250HBW(25HRB) |
ASTM A213 Tabung Baja ing njaba Diameter lan Toleransi Kekandelan Tembok
OD, mm | OD Toleransi |
< 25.4 | +/- 0,10 |
25.4 – <= 38.1 | +/- 0,15 |
> 38.1 -< 50.8 | +/- 0,20 |
50.8 -< 63.5 | +/- 0,25 |
63.5 -< 76.2 | +/- 0.30 |
76.2 – <= 101.6 | +/- 0,38 |
> 101.6 – <= 190.5 | +0.38/-0.64 |
> 190.5 – <= 228.6 | +0.38/-1.14 |
OD, mm | Toleransi WT |
<= 38.1 | +20%/-0 |
> 38.1 | +22%/-0 |
Cakupan Standar ASTM A213
1.1 Spesifikasi iki nyakup boiler baja feritik lan austenitik sing mulus, superheater, lan tabung penukar panas, Kelas T91, TP304, lsp. Baja iki kadhaptar ing Tabel 1 lan 2.
1.2 Gelar sing ngemot huruf, H, ing sebutane, nduweni syarat sing beda karo sing padha ora ngemot huruf, H. Syarat sing beda-beda iki nyedhiyakake kekuatan creep-rupture sing luwih dhuwur tinimbang sing bisa ditindakake ing kelas sing padha tanpa syarat sing beda-beda.
1.3 Ukuran pipa lan kekandelan biasane diwenehake kanggo spesifikasi iki yaiku 1/8 in. [3,2 mm] diametere njero nganti 5 in. [127 mm] diameter njaba lan 0,015 nganti 0,500 in. [0,4 nganti 12,7 mm], kalebu, ing kekandelan tembok minimal utawa, yen kasebut ing urutan, kekandelan tembok rata-rata.Tubing sing duwe diameter liyane bisa uga dilengkapi, yen tabung kasebut tundhuk karo kabeh syarat liyane saka spesifikasi iki.
1.4 Nilai sing kasebut ing siji unit SI utawa unit inch-pound kudu dianggep minangka standar.Ing teks, unit SI ditampilake ing kurung.Nilai sing kasebut ing saben sistem bisa uga ora padha;mulane, saben sistem bakal digunakake independen saka liyane.Gabungan nilai saka rong sistem bisa nyebabake ora cocog karo standar kasebut.Unit inch-pound kudu ditrapake kajaba sebutan "M" saka spesifikasi iki ditemtokake ing urutan kasebut.
Tabel 1 Watesan Komposisi Kimia,% A, kanggo Low Alloy SteelA Maksimum, kajaba sawetara utawa minimal dituduhake.Ing ngendi elips (...) katon ing tabel iki, ora ana syarat, lan analisis unsur ora perlu ditemtokake utawa dilapurake.
B Diijini pesen T2 lan T12 kanthi kandungan belerang maksimal 0,045..
C Utawa, minangka pengganti rasio minimal iki, materi kudu kekerasan minimal 275 HV ing kondisi hardened, ditetepake minangka sawise austenitizing lan cooling kanggo suhu kamar nanging sadurunge tempering.Pengujian kekerasan kudu ditindakake ing tengah kekandelan produk.Frekuensi uji kekerasan kudu dadi rong conto produk saben lot perawatan panas lan asil uji kekerasan kudu dilaporake ing laporan uji materi.
Lumahing dicet ireng, dilapisi PE