ASTM A53 / A106 Pipa Seamless
ASTM A53 pipa baja karbon nyertakeun seamless, dilas, hideung, sarta panas-dipped pipe galvanized.
Standar | BS 1387, BS EN 10297, BS 4568, BS EN10217, JIS G3457 |
Kelas | 10#-45#, Cr-Mo alloy, 15NiCuMoNb5, 10Cr9Mo1VNb, A53-A369 |
Diaméterna kaluar | 21,3 - 610 mm |
Kandel témbok | 2 - 50 mm |
Bentuk Bagéan | Buleud |
Aplikasi | Pipa Cairan |
Perlakuan permukaan | varnished, cap, nyirian |
Sertifikasi | API |
Pipa Baja Karbon | ASTM A53/106/API 5L B |
ST37 / ST44 Precision Pipa Steel Seamless | DIN 2448/2391/1629/17100 |
DIN 2391/2448/1629, ST37 / ST52 pipa baja | ST37/ST52 |
Hot Rolled Pipa Steel Seamless | ASTM A 53/106/API 5L B |
Tiis Digambar Seamless Steel Boiler Tube | ASTM A106/DIN 17175/2448 |
Karbon Seamless Steel Pipa | ASTM A53/106/API 5L B |
ASTM A53 pipa baja karbon nyertakeun seamless, dilas, hideung, sarta panas-dipped pipe galvanized.
ASTM A53 KELAS A&B
spésifikasi ieu nyertakeun mulus tur dilas hideung jeung panas-dipped pipa baja galvanized dina ukuran nominal 1/8”ka 20 di inklusif (3.18mm-660.4mm) kalawan nominal (rata) ketebalan témbok.
ASTM A106 KELAS A, B & C
spésifikasi ieu nyertakeun pipe baja karbon seamless pikeun layanan suhu luhur dina ukuran nominal 1/8 di. Ka 26 di inklusif (3.18mm-660.4mm) kalawan nominal (rata) ketebalan témbok.
Kelas A Karbon 0,25% max.Mangan 0,27 nepi ka 0,93%
Kelas B Karbon 0,30% max.Mangan 0,29 nepi ka 1,06%
Kelas C Karbon 0,35% max.Mangan 0,29 nepi ka 1,06%
Sadaya sasmita gaduh nilai anu sami pikeun Walirang 0,058% maksimal.Fosfor 0,048% max.Silikon 0,20% mnt.
Komposisi Kimia (%):
Standar | Kelas | C | Si | Mn | P | S | Ni | Cr | Cu | Mo | V |
ASTM A53M | A | =0.25 | - | = 0,95 | =0.05 | = 0,045 | =0.40 | =0.40 | =0.40 | =0.15 | =0.08 |
B | =0.30 | - | =1.2 | =0.05 | = 0,045 | =0.40 | =0.40 | =0.40 | =0.15 | =0.08 |
Sipat mékanis:
Standar | Kelas | Kakuatan tegangan (Mpa) | kakuatan ngahasilkeun (Mpa) | Elongation (%) | |
ASTM A53M | A | =330 | =205 | Tempo tabél 3 ASTM A53 | |
Standar | Kelas | C | Si | Mn | P | S | Ni | Cr | Cu | Mo | V |
ASTMA106M | A | =0.25 | =0.10 | 0.27-0.93 | = 0,035 | = 0,035 | =0.40 | =0.40 | =0.40 | =0.15 | =0.08 |
B | =0.30 | =0.10 | 0.29-1.06 | = 0,035 | = 0,035 | =0.40 | =0.40 | =0.40 | =0.15 | =0.08 | |
C | =0.35 | =0.10 | 0.29-1.06 | = 0,035 | = 0,035 | =0.40 | =0.40 | =0.40 | =0.15 | =0.08 |
Sipat mékanis:
Standar | Kelas | Kakuatan tegangan (Mpa) | kakuatan ngahasilkeun (Mpa) | Elongation (%) |
ASTM A106M | A | =330 | =205 | Tempo tabél 4 ASTM A106 |
B | =415 | =240 | ||
C | =485 | =275 |
varnished, cap, nyirian