EN 10216: Standards tal-UE

EN 10216-1: Standards tal-UE
EN 10216-2: Standards tal-UE

 

Għan:
Għall-bojlerpajpijiet, pajpijiet tat-tabakk, tubi super heater, tubi pre-heater ta 'l-arja.

Wara konsultazzjonijiet, jistgħu wkoll jiġu provvista gradi oħra ta ' pajp ta ' l-azzar.

Proprjetajiet mekkaniċi:

Standard

Grad

Saħħa tat-tensjoni (MPa)

Qawwa ta' rendiment (MPa)

Titwil (%)

EN10216-1

P195

320440

≥195

≥27

P235

360500

≥235

≥25

P265

410570

≥265

≥23

EN10216-2

P195GH

320440

≥195

≥27

P235GH

360500

≥235

≥25

P265GH

410570

≥265

≥23

13CrMo4-5

440590

≥290

≥22

10CrMo9-10

480630

≥280

≥22

Kompożizzjoni kimika:

Standard

Grad

Kompożizzjoni Kimika

C

Si

Mn

P

S

Cr

Mo

Cu

Ni

V

EN10216-1

P195

≤0.13

≤0.35

≤0.70

≤0.025

≤0.020

≤0.30

≤0.06

≤0.30

≤0.30

/

P235

≤0.16

≤0.35

≤1.20

≤0.025

≤0.020

≤0.30

≤0.06

≤0.30

≤0.30

/

P265

≤0.20

≤0.40

≤1.40

≤0.025

≤0.020

≤0.30

≤0.06

≤0.30

≤0.30

/

EN10216-2

P195GH

≤0.13

≤0.35

≤0.70

≤0.025

≤0.020

≤0.30

≤0.06

≤0.30

≤0.30

/

P235GH

≤0.16

≤0.35

≤1.20

≤0.025

≤0.020

≤0.30

≤0.06

≤0.30

≤0.30

/

P265GH

≤0.20

≤0.40

≤1.40

≤0.025

≤0.020

≤0.30

≤0.06

≤0.30

≤0.30

/

13CrMo4-5

0.100.17

≤0.35

0.400.70

≤0.025

≤0.020

0.701.15

0.400.60

≤0.30

≤0.30

/

10CrMo9-10

0.080.14

≤0.50

0.300.70

≤0.025

≤0.020

2.002.50

0.901.10

≤0.30

≤0.30

/


Ħin tal-post: Ġunju-07-2022