ASTM A234 se Standard Spesifikasyon pou ekipman tiyo asye gen ladan materyèl kabòn ak alyaj asye pou sèvis tanperati modere ak segondè.Li kouvri ekipman asye nan kalite san pwoblèm ak soude.Fittings Steel tiyo yo aplike nan tiyo presyon ak nan fabrikasyon veso presyon.Materyèl ekipman sa yo konpoze de asye touye, forgings, ba, plak, san pwoblèm oswa HFW (fusion soude) pwodwi tiyo, ak metal filler ajoute.
ki sa ki WPB?
W = WELDABLE / fòje
P = ki gen rapò ak P KANTITE MATERYÈL ALOYY
B = REFERE A MINIMÒM RENDEMENT MATERYÈL
Yo disponib nan dènye revizyon ASME B16.9, B16.11, MSS-SP-79, MSS-SP-83, MSS-SP-95, ak MSS-SP-97.Epitou lajman itilize nan tiyo presyon ak nan fabwikasyon veso presyon pou sèvis nan tanperati modere ak ki wo.Klas yo se ASTM A234 WPB, WPC, WP5, WP9, WP91, WP11, WP12 ak WP22.
Espesifikasyon:
Estanda: ANSI / ASME B16.9, B16.28, MSS-SP-43.
Dyamèt eksteryè ranje: 1/2 "a 48"
Ranje epesè: SCH 10, sch 20, SCH 40, SCH STD, SCH 80, SCH XS, SCH 160, SCH XXS elatriye.
Fittings asye tiyo fabrikasyon kalite nan fòje, threaded, soude bou, ak san pwoblèm.
Konpozisyon chimik (%) ASTM A234
Klas | C | Mn | P | S | Si | Cr | Mo | Ni | Cu | V | Nb |
WPB | 0.3 | 0.29-1.06 | 0.05 | 0.058 | 0.1min | 0.4 | 0.15 | 0.4 | 0.4 | 0.08 | 0.02 |
WPC | 0.35 | 0.29-1.06 | 0.05 | 0.058 | 0.1min | 0.4 | 0.15 | 0.4 | 0.4 | 0.08 | 0.02 |
WP11 CL1 | 0.05-0.15 | 0.30-0.60 | 0.03 | 0.03 | 0.50-1.00 | 1.00-1.50 | 0.44-0.65 | - | - | - | - |
WP11 CL2/3 | 0.05-0.20 | 0.30-0.80 | 0.04 | 0.04 | 0.50-1.00 | 1.00-1.50 | 0.44-0.65 | - | - | - | - |
Pwopriyete mekanik ASTM A234
Kondisyon pou Tensile | WPB | WPC, WP11CL2 | WP11CL1 | WP11CL3 |
Fòs Tensile, min, ksi[MPa] | 60-85 | 70-95 | 60-85 | 75-100 |
(0.2% konpanse oswa 0.5% ekstansyon-anba-chaj) | [415-585] | [485-655] | [415-585] | [520-690] |
Fòs Sede, min, ksi[MPa] | 32 | 40 | 30 | 45 |
[240] | [275] | [205] | [310] |
A234 WPB ekivalan
Tiyo | Fittings | Bride | Tiyo | Boulon & Pistach |
ASTM A106 Gr A | ASTM A234 Gr WPA | ASTM A105 | ASTM A216 Gr WCB | A193 Gr B7 A194 Gr 2H |
ASTM A106 Gr B | A234 Gr WPB | ASTM A105 | ASTM A216 Gr WCB | |
ASTM A106 Gr C | ASTM A234 Gr WPC | ASTM A105 | ASTM A216 Gr WCB |
(1) Sòm Cu, Ni, Cr, ak Mo pa dwe depase 1.00%.
(2) Sòm Cr ak Mo pa dwe depase 0.32%.
(3) Pou chak rediksyon 0.01% pi ba pase C max espesifye a, yon ogmantasyon de 0.06% Mn (4)pi wo pase max espesifye a.yo pral pèmèt, jiska yon max.de 1.35%.
(5) Max.ekivalan kabòn (CE) dwe 0.50, ki baze sou analiz chalè ak (6) fòmil CE=C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15.
Diferans ki genyen ant A105 ak A234
ASTM A234 WPB tiyo Fittings yo te fè leve nan asye kabòn fòje ke yo trè fò epi yo ka aplike nan kondisyon ki gen gwo fòs.ASTM A234 WPB yo trete chalè epi yo pèmèt yo refwadi rapidman.
Carbon Steel Forged Fittings yo se ekipman tiyo ki fèt ak materyèl A105.Sa yo pwodui nan kondisyon rkwit, nòmalize, nòmalize ak tanperaman oswa trempe ak tanperaman.
Tan poste: Oct-08-2021